Die Materialien der Sinter-Kamin-Bar:
Chemical composition |
C |
Si |
Mn |
P |
S |
Cr |
Ni |
Content |
1.0~1.6 |
≤1.50 |
≤1.20 |
≤0.05 |
≤0.05 |
23~28 |
0.6~1.2 |
Merkmale von Sinter-Kamin-Bar
Mechanical index |
Standard requirement |
Mechanical index |
Standard requirement |
Mechanical index |
Standard requirement |
Tensile strength (kgf/mm2) |
Min 50 |
Impact energy Aku, kgf.m/cm2 |
Min0.25 |
Shore hardness |
Min 40 |
Wir können es gemäß der Zeichnung herstellen.
OEM casting |
According to the customer`s drawing and requirements |
Course of production |
Model making→Molding/Core→Mold assembling→Melting→Pouring→Opening→Finishing→Heat treatment→Non-destructive→Inspection→Welding→Test |
Standard |
GB/1135.2-89 |
Casting process |
Sodium silicate sand, Resin sand |
Our Material |
Plain carbon steel, Low alloy steel, High manganese steel, High chromium cast iron(No more than 35 tons) |
Surface treatment |
Anti-rust oil, powder coating, epoxy spray coating, anodic oxidation treatment, plating or as per requirements |
Packaging |
Wooden case, crate, parcel, bale, package, barrel, etc. |